he electrochemical behavior and surface analysis of i 50 Ni 47 . 2 Co 2 . 8 alloy for orthodontic use

@inproceedings{Wanga2008heEB,
  title={he electrochemical behavior and surface analysis of i 50 Ni 47 . 2 Co 2 . 8 alloy for orthodontic use},
  author={Yu-zhong Wanga and Yuanjin Zhenga},
  year={2008}
}
Objectives. The aim of this study was to investigate the electrochemical behavior of Ti50Ni47.2Co2.8 alloy in deaerated artificial saliva solutions with binary NiTi alloy as reference and to characterize the composition and structure of the passive film after polarization tests. Methods. The corrosion behavior of NiTiCo alloy was systematically studied by open circuit potential, potentiodynamic and potentiostatic techniques. The surface characterization after anodic polarization tests were… CONTINUE READING