Viscous flow behavior of four iron-containing silicates with alumina, effects of composition and oxidation condition.

@inproceedings{Klein1983ViscousFB,
  title={Viscous flow behavior of four iron-containing silicates with alumina, effects of composition and oxidation condition.},
  author={Lisa C. Klein and B. V. Fasano and Jenn Ming Wu},
  year={1983}
}
The viscosity of four iron-containing silicates with alumina has been measured under oxidizing and reducing conditions over the temperature range 450° to 700°C. Initially, the compositions contain approximately 2, 5, 10, and 20 mol.% of trivalent metal oxide. The viscosities of compositions with approximately equimolar Fe3+ and Al3+ are compared to those determined for compositions with trivalent cation all Fe or all Al. Then the batch composition calculated to replace one half of the Fe3+ by… CONTINUE READING