The thermal decomposition of commercial silicone grease was carried out in a closed reactor (Swagelok) that was heated at 800 degrees C for 3 h, yielding a SiO2-carbon composite with a BET surface area of 369 m2/g. The bulk conductivity (5.72 x 10(-6) S x cm(-2)) of the SiO2-carbon composite was determined by impedance measurements. The as-prepared SiO2… (More)