Some mechanistic observation on water-deteriorated dental composite resins.

Abstract

Four different types of dental composite resins were subjected to the water sorption environment in both dyed and undyed distilled water for 1 and 5 weeks at 37 degrees C. Weight changes due to the water sorption, effects of water sorption on mechanical properties, and fractographic observations were conducted. It was found that (i) the water sorption was… (More)