          641-6
        }
}
The preparation of hollow hydroxyapatite (HA) microspheres as potential drug-delivery vehicles was investigated. A lithium-calcium-borate (10Li(2)O-15CaO-75B(2)O(3)) (mol%) glass, made by fusing the components at 1100 degrees C for 1 h, was ground to a powder and passed through a flame at approximately 1400 degrees Celsius to spheroidize the particles. The resulting glass microspheres (106-125 microm in diameter) were reacted in 0.25 M K(2)HPO(4) solution for 5 days at 37 degrees Celsius and pH… CONTINUE READING