Measurement and evaluation of galvanic corrosion between titanium/Ti6A14V implants and dental alloys by electrochemical techniques and auger spectrometry.

@article{Grosgogeat1999MeasurementAE,
  title={Measurement and evaluation of galvanic corrosion between titanium/Ti6A14V implants and dental alloys by electrochemical techniques and auger spectrometry.},
  author={Brigitte Grosgogeat and Lucien Reclaru and Mich{\`e}le Lissac and Francis Dalard},
  journal={Biomaterials},
  year={1999},
  volume={20 10},
  pages={933-41}
}
The purpose of this study was to investigate, in different experimental conditions, the galvanic corrosion phenomena which can exist between a dental suprastructure and a dental implant. The electrochemical behavior of 7 alloy superstructures with titanium and titanium alloy (Ti6A14V) implants was investigated by electrochemical means in Fusayama-Meyer de-aerated saliva and Carter-Brugirard (AFNOR) non de-aerated saliva. Different techniques were used to obtain the value of the galvanic… CONTINUE READING

Citations

Publications citing this paper.
Showing 1-10 of 25 extracted citations

Similar Papers

Loading similar papers…