Influence of stress corrosion on the mechanical properties of laser-welded titanium.

Abstract

STATEMENT OF PROBLEM Whether laser-welded (LW) titanium can resist the stress corrosion produced by the combination of fluoride ions and stress in the oral environment is unknown. PURPOSE The purpose of this in vitro study was to investigate the influence of stress corrosion on the mechanical properties of LW titanium. MATERIAL AND METHODS Twenty-seven… (More)
DOI: 10.1016/j.prosdent.2015.09.002

Topics

Cite this paper

@article{Ferreira2016InfluenceOS, title={Influence of stress corrosion on the mechanical properties of laser-welded titanium.}, author={Nancy de Assis Ferreira and Pl{\'i}nio Mendes Senna and Dalva Cristina Baptista do Lago and Lilian Ferreira de Senna and Helio Rodrigues Sampaio-Filho}, journal={The Journal of prosthetic dentistry}, year={2016}, volume={115 3}, pages={356-62} }