Full densification of Molybdenum powders using Spark Plasma Sintering


Pure molybdenum powder was sintered using Spark Plasma Sintering under various temperatures, and holding times, under a pressure of 77 MPa and a heating rate at 700°C/min. After sintering, a carbide layer was observed at the surface. The carbide layer thickness, the relative density of the sample as well as the microhardness and the grain size of Mo were… (More)