Fabrication tolerances in As2S3 negative-curvature antiresonant fibers

Abstract

We computationally investigate fabrication tolerances in As2S3 negative-curvature antiresonant tube-lattice fibers. Since the dominant loss mechanisms for silica in the mid-infrared (mid-IR) is material absorption, As2S3, which offers a reduced loss over that wavelength range, is a natural candidate for mid-IR antiresonant fibers. However, any fiber… (More)

Topics

8 Figures and Tables

Cite this paper

@inproceedings{Weiblen2016FabricationTI, title={Fabrication tolerances in As2S3 negative-curvature antiresonant fibers}, author={R. Joseph Weiblen and Curtis R. Menyuk and Rafael R. Gattass and L. Brandon Shaw and Jasbinder Singh Sanghera}, year={2016} }