Effects of Sintering Temperature on Crystallization and Fabrication of Porous Bioactive Glass Scaffolds for Bone Regeneration

Abstract

In this work the sintering ability of borosilicate (S53B50), borophosphate (P40B10) and phosphate (Sr) bioactive glasses was investigated. The glass powders were crushed and sintered in air at a heating rate of 10 °C/min for 2 hours at sintering temperatures between 480 °C–600 °C. The aim was to define the optimum sintering temperature prior to glass… (More)
DOI: 10.1038/s41598-017-06337-2