Comparison of galvanic corrosion potential of metal injection molded brackets to that of conventional metal brackets with nickel-titanium and copper nickel-titanium archwire combinations.

@article{Varma2013ComparisonOG,
  title={Comparison of galvanic corrosion potential of metal injection molded brackets to that of conventional metal brackets with nickel-titanium and copper nickel-titanium archwire combinations.},
  author={D. P. Varma and S. Chidambaram and K. B. Reddy and M. Vijay and D. Ravindranath and M. R. Prasad},
  journal={The journal of contemporary dental practice},
  year={2013},
  volume={14 3},
  pages={
          488-95
        }
}
  • D. P. Varma, S. Chidambaram, +3 authors M. R. Prasad
  • Published 2013
  • Medicine, Materials Science
  • The journal of contemporary dental practice
  • AIM The aim of the study is to investigate the galvanic corrosion potential of metal injection molding (MIM) brackets to that of conventional brackets under similar in vitro conditions with nickel-titanium and copper nickel-titanium archwires. MATERIALS AND METHODS Twenty-five maxillary premolar MIM stainless steel brackets and 25 conventional stainless steel brackets and archwires, 0.16 inch, each 10 mm length, 25 nickeltitanium wires, 25 copper nickel-titanium wires were used. They were… CONTINUE READING