Minority carrier lifetime was determined by MW-PCD method following the industry process well and truly. The wafer as-cut without any treatment showed an effective lifetime about 1.2μs. Then it rose to 2.5∼5μs after one side was passivated by silicon nitride. The average lifetime with double layer passivation sharply increased to(More)