Single crystalline Sn doped In(2)O(3) (ITO) NWs (nanowires) were synthesized via an Au-catalyzed VLS (vapor-liquid-solid) method at 600 °C. The different sizes (~20, ~40, ~80 nm) of the Au NPs (nanoparticles) provided the controllable diameters for ITO NWs during growth. Phase and microstructures confirmed by high-resolution transmission electron microscope(More)
Selective area growth of single crystalline Sn-doped In2O3 (ITO) nanowires synthesized via vapor-liquid-solid (VLS) method at 600°C was applied to improve the field emission behavior owing to the reduction of screen effect. The enhanced field emission performance reveals the reduction of turn-on fields from 9.3 to 6.6 V μm-1 with increase of field(More)