Hydrogen produced by reforming of fossil fuel would be preferable in early stage of proton exchange membrane (PEM) fuel cell operation. Impurities other than hydrogen could cause catalyst poisoning and fuel cell performance degradation. Hydrogen produced by reformation process include about 2% methane. The presence of methane up to 10% is reported(More)