SnO2 thin films were fabricated using low-pressure thermal chemical vapor deposition. The results of X-ray photoelectron spectroscopy revealed that the SiO2 layer with an O1S-binding energy of 531.2 eV was formed before the SnO2 layer with an O1S-binding energy of 530.5 eV was formed. In the beginning, the SnO2 thin film showed Sn3d5-binding energy peaks of(More)
In this study, C-doped TiO2 particles were successfully synthesized by a hydrothermal method. Three binding energy peaks were observed at 284.6, 286.2, and 288.5 eV in the C is region of the XPS. The signals at 286.2 and 288.5 eV were attributed to chemically bound C-O and Ti-C-O linkages within the crystalline TiO2 lattice, respectively. The introduction(More)