Dicing of ultrathin (e.g. <; 75um thick) “via-middle” 3DI/TSV semiconductor wafers proves to be challenging because the process flow requires the dicing step to occur after wafer thinning and back side processing. This eliminates the possibility of using any type of “dice-before-grind” techniques. In addition, the presence of(More)