Poly(D,L-lactide) synthesis using tin(II) 2-ethylhexanoate initiated ring-opening polymerization (ROP) takes over 30 hours in bulk at 120 °C. The use of microwave makes the same bulk polymerization process with the same initiator much faster and energy saving, with a reaction time of about 30 minutes at 100 °C. Here, the poly(lactide) synthesis was done in(More)