Ishwar Prasad Sahu

Learn More
Ca2MgSi2O7:Eu(2+),Dy(3+) phosphor was prepared by the solid-state reaction method under a weak reducing atmosphere. The obtained phosphor was characterized using X-ray diffraction (XRD), transmission electron microscopy (TEM), field emission scanning electron microscopy (FESEM), energy dispersive X-ray spectroscopy (EDX) and Fourier transform infrared(More)
Copper-doped zinc sulfide (ZnS:Cu) nanoparticles with varying concentrations of capping agent were prepared using a chemical route technique. These particles were characterized by scanning electron microscopy (SEM), transmission electron microscopy and X-ray diffraction (XRD). Optical absorption studies showed that the absorption edge shifted towards the(More)
In this work, we report the synthesis of Y2O3:Er(3+), Y2O3:Yb(3+) and Y2O3:Er(3+),Yb(3+) nanophosphors by the combustion synthesis method using urea as fuel. The doping agents were incorporated in the form of erbium nitrate and ytterbium nitrate. X-Ray diffraction (XRD) patterns revealed that the synthesized particles have a body-centered cubic structure(More)
A series of Ce3+ ion single-doped Ca2 Al2 SiO7 phosphors was synthesized by a combustion-assisted method at an initiating temperature of 600 °C. The samples were annealed at 1100 °C for 3 h and their X-ray diffraction patterns confirmed a tetragonal structure. The phase structure, particle size, surface morphology and elemental analysis were analyzed using(More)
A europium (Eu)-doped di-calcium magnesium di-silicate phosphor, Ca2MgSi2O7 :Eu(2+) , was prepared using a solid-state reaction method. The phase structure, particle size, surface morphology, elemental analysis, different stretching mode and luminescence properties were analyzed by X-ray diffraction (XRD), transmission electron microscopy (TEM), field(More)
In the present article we report europium-doped strontium ortho-silicates, namely Sr2 SiO4 :xEu3+ (x = 1.0, 1.5, 2.0, 2.5 or 3.0 mol%) phosphors, prepared by solid state reaction method. The crystal structures of the sintered phosphors were consistent with orthorhombic crystallography with a Pmna space group. The chemical compositions of the sintered(More)
Sr2MgSi2O7:Eu(2+) and Sr2MgSi2O7:Eu(2+),Dy(3+) long afterglow phosphors were synthesized under a weak reducing atmosphere by the traditional high temperature solid state reaction method. The synthesized phosphors were characterized by powder X-ray diffraction (XRD), energy dispersive X-ray spectroscopy (EDX), and photo-, thermo- and mechanoluminescence(More)
Ca2 MgSi2 O7 :Ce3+ , Ca2 MgSi2 O7 :Eu2+ and Ca2 MgSi2 O7 :Eu2+ ,Ce3+ phosphors were prepared using the solid-state reaction method. The crystal structures of the sintered phosphors were of melilite type, which has a tetragonal crystallography. The chemical compositions of the sintered phosphors was confirmed by energy dispersive X-ray spectroscopy. The(More)