PURPOSE To evaluate the microshear bond strength (μSBS) of several universal adhesive systems applied on five different indirect restorative materials. MATERIALS AND METHODS Five CAD/CAM materials were selected: 1) indirect resin composite (LAV); 2) feldspathic glass ceramic (VTR); 3) leucite-reinforced glass-ceramic (EMP); 4) lithium disilicate ceramic(More)
INTRODUCTION This article presents a 6-month case report and an in vitro evaluation of the performance of the new self-etching glass-ceramic monobond etch and prime (MEP) when applied in a lithium disilicate (LD). The MEP contains in the same bottle, along with acid conditioner and silanes. This simplifies the bonding procedures by reducing not only the(More)
PURPOSE To evaluate the effect of a silane and an adhesive containing MDP, used alone or combined in the same solution, on the microshear bond strength (μSBS) to lithium disilicate ceramics immediately and after 1-year water storage, and compare the bond strength results with the Raman spectra of the treated lithium disilicate surfaces. MATERIALS AND(More)
  • 1